Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1449 MPa | 210200 psi | |
HP Alloys Alloy C-276, 50% Cold Worked 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |