Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.666 MPa | 1402 psi | post cured- 8 hours at 166°C; ASTM D412 |
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |