Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.3 MPa | 2070 psi | ASTM D412 |
Multibase Multi-Flex® TPE G 7680 NAT The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 14.3 - 50.3 MPa | 2080 - 7300 psi | Average value: 38.0 MPa Grade Count:56 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 14.3 MPa | 2080 psi | ASTM D412 |
R70-058 Styrene-based Biomedical Elastomer |