Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.0965266 - 0.0965266 MPa

@Temperature 18.3 - 149 °C
14.0000 - 14.0000 psi

@Temperature 65.0 - 300 °F
Average value: 0.0965 MPa Grade Count:1
Overview of materials for Methacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri..