Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 703 - 945 MPa | 102000 - 137000 psi | |
Kobe Steel KS15-3-3-3 Beta Titanium Alloy, AMS 4914, Solution treated Nominal Composition: Ti-15 V-3 Cr-3 Sn-3 AlApplications: Aircraft parts, bicycle gears, gold club heads, foils. Features:Cold workable.Information provided by Kobe Steel |