Polymer Property : Tensile Strength, Ultimate = 1370 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.45 MPa
1370 psi
no post cure, press cured for 5 minutes; ASTM D412
Multibase SILASTIC® Q7-4840 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tensile Strength, Ultimate 9.45 MPa
1370 psi
Dow Corning SILASTIC® LS 5-8750 FLUOROSILICONE RUBBER
33 durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Tensile Strength, Ultimate 9.45 MPa
1370 psi
Dow Corning SILASTIC® Q7-4840 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning
Tensile Strength, Ultimate 9.45 MPa
1370 psi
ASTM D412
3M 8560 Cold Shrink Silicone Rubber 3/C Cable Breakout Boots
The 3M cold Shrink Silicone Rubber 3/C Cable Breakout Boots 8560 Series are a series of open-ended molded silicone rubber sealing assemblies that are factory expanded and mounted on removable inner ..