Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1370 MPa | 198000 psi | |
Kinetics MIM 420 Stainless Steel (Oil Quench Heat Treat) Martensitic stainless steel. Very good strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Higher hardness typical with oil quench over that of vacuum heat t.. |
|||
Tensile Strength, Ultimate | 1370 MPa @Temperature 650 °C |
199000 psi @Temperature 1200 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 1370 MPa | 199000 psi | |
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co.. |