Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1240 - 1340 MPa | 180000 - 195000 psi | |
Materion BrushCAST® 275CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Ultimate | 1240 - 1340 MPa | 180000 - 195000 psi | |
Materion BrushCAST® 275C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |