Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1336 MPa | 193800 psi | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Tensile Strength, Ultimate | 1336 MPa | 193800 psi | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 35% Cold Reduction Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |