Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.10 MPa | 1320 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 8103 BLK Multi-Flex® A 8103 is a moderately low price TPE that has a god tensile and tear strength as well as very good elasticity. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 9.100 MPa @Temperature 23.0 °C |
1320 psi @Temperature 73.4 °F |
ASTM Reference Fuel B Immersion, 168 hours; ASTM D1414 |
Freudenberg Simrit N470 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Tensile Strength, Ultimate | 9.10 MPa | 1320 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |