Polymer Property : Tensile Strength, Ultimate = 13.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.3 MPa
1930 psi
Freudenberg Simrit V189 Non-Black Compound
Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p..
Tensile Strength, Ultimate 13.3 MPa
1930 psi
Freudenberg Simrit V75BR Non-Black Compound
Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p..