Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 129 MPa

@Temperature 982 °C
18700 psi

@Temperature 1800 °F
Haynes HR-160® alloy, solution annealed sheet
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..