Tensile Strength, Ultimate 8.791 MPa
1275 psi
Dow Corning S50 LIQUID SILICONE RUBBER KIT
A heat-cured elastomer for use by customers fabricating medical devices, including those intended for implantation in humans for less than 30 days and non-implant applications. Dow Corning® S50 Liq..