Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1275 MPa | 184900 psi | when tempered around 950°F |
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02) An oil-hardening alloy with excellent size change properties, Stentor tool steel is especially suited for general purpose work in the toolroom. It is safe to harden, and shows little size change or .. |