Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1268 MPa
183900 psi
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi..
Tensile Strength, Ultimate 1268 MPa

@Temperature -73.0 °C
183900 psi

@Temperature -99.4 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..