Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1224 MPa | 177500 psi | Hardened 1900°F, Tempered 1000°F |
ATI Allegheny Ludlum 440A Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 1224 MPa | 177500 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 538°C Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |