Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.40471 - 25.7933 MPa @Temperature 93.3 - 275 °C |
1219.00 - 3741.01 psi @Temperature 200 - 527 °F |
Average value: 17.8 MPa Grade Count:16 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Ultimate | 8.40471 - 25.7933 MPa @Time 86400 - 3.60e+6 sec |
1219.00 - 3741.01 psi @Time 24.0 - 1000 hour |
Average value: 17.8 MPa Grade Count:16 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |