Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 836.3 MPa | 121300 psi | |
Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 2150°F (1180°C) + Aged 1400°F (760°C) Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 2150°F (1180°C)/5 minutes/AC + Aged 1400°F (760°C)/100h/AC. This produces ASTM grain siz.. |