Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1000 - 1200 MPa | 145000 - 174000 psi | |
SSAB Tunnplat Docol® 1000 DL High-strength Steel In course of development.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Ultimate | 1000 - 1200 MPa | 145000 - 174000 psi | |
SSAB Tunnplat Docol® 1000 DP High-strength Steel High-strength SteelCharacteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is.. |
|||
Tensile Strength, Ultimate | 1000 - 1200 MPa | 145000 - 174000 psi | as built |
EOS MS1 Maraging Steel for DMLS 3D Printing EOS Maraging Steel MS1 is a steel powder which has been optimized especially for processing on EOSINT M 270 systems. This steel has very good mechanical properties, and is easily heat-treatable us.. |
|||
Tensile Strength, Ultimate | 1100 - 1200 MPa | 160000 - 174000 psi | as built, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Tensile Strength, Ultimate | 1100 - 1200 MPa | 160000 - 174000 psi | |
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Precipitation Heat Treated, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Ultimate | 980 - 1200 MPa | 142000 - 174000 psi | |
ArcelorMittal Complex Phase Steel 1000 SF Very high strength steel, Cold Rolled Steel Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels are cold formed to make lightweight structural elements. A num.. |
|||
Tensile Strength, Ultimate | 980 - 1200 MPa | 142000 - 174000 psi | |
ArcelorMittal Complex Phase Steel 1000 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT980C) and electrogalvanized (HCT980C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |