Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 0.829 MPa
>= 120 psi
ASTM D3574E
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam
Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo..
Tensile Strength, Ultimate 0.827 MPa
120 psi
cured 30 days @ 25°C
Abatron AboCast 8110-1/AboCure 8110-2 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..
Tensile Strength, Ultimate >= 0.829 MPa
>= 120 psi
ASTM D3574E
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..