Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.65 MPa
1110 psi
ASTM D638
Colorite Polymers 3511-02 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..