Polymer Property : Tensile Strength, Ultimate = 107400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 740.5 MPa
107400 psi
Typical Annealed
Special Metals INCONEL® C276 Nickel Superalloy Plate
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia..