Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.40 MPa
1070 psi
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound &
Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. ..
Tensile Strength, Ultimate 7.36 - 191.87 MPa

@Temperature -40.0 - 150 °C
1070 - 27828 psi

@Temperature -40.0 - 302 °F
Average value: 61.4 MPa Grade Count:2
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Tensile Strength, Ultimate 7.36 - 191.87 MPa

@Strain 0.180 - 160 %
1070 - 27828 psi

@Strain 0.180 - 160 %
Average value: 61.4 MPa Grade Count:2
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Tensile Strength, Ultimate 7.40 MPa
1070 psi
Kuraray SEPTON® S45 Soft Compound
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre..
Tensile Strength, Ultimate 7.35 MPa
1070 psi
ASTM D412
Stellarchem SV-B70E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Tensile Strength, Ultimate 7.40 - 31.8 MPa
1070 - 4610 psi
Average value: 19.3 MPa Grade Count:42
Overview of materials for Chlorosulfonated Polyethylene Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val..