Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1060 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.31 MPa
1060 psi
post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4565 DICUP R Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 7.30 MPa
1060 psi
Freudenberg Simrit S40GY Silicone Elastomer
Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b..
Copyright © lookpolymers.com All Rights Reserved