Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.128 MPa | 1034 psi | After 7 days at 70°C; ASTM D412 ISO 37 |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |