Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 10.3421 - 13.7895 MPa @Temperature 100 - 121 °C |
1500.00 - 2000.00 psi @Temperature 212 - 250 °F |
Average value: 12.0 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 10.3421 - 13.7895 MPa @Time 605000 - 605000 sec |
1500.00 - 2000.00 psi @Time 168 - 168 hour |
Average value: 12.0 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |