Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.10 MPa | 160 psi | ASTM D 638 |
REXtac Rextac® RT 2280 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and high viscosityApplications: Component of hot melt adh.. |
|||
Tensile Strength, Ultimate | 1.10 MPa | 160 psi | |
Kuraray HYBRAR® F4 Foam Compound Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |