Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.896 MPa | 130 psi | |
Dow Corning 1437 INDUSTRIAL SEALANT AND ADHESIVE Neutral Cure RTV SealantInformation provided by Dow Corning |
|||
Tensile Strength, Ultimate | 0.896 MPa @Temperature 204 °C |
130 psi @Temperature 400 °F |
|
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber) Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin.. |