Polymer Property : Tensile Strength, Ultimate = 0.610 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.610 MPa
88.5 psi
ASTM D 638
REXtac Rextac® RT 2730 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good track, and very long open timeApplications: Component of hot me..
Tensile Strength, Ultimate 0.610 MPa
88.5 psi
ASTM D 638
REXtac Rextac® RT 4730 Amorphous Polyalphaolefin (APAO)
Wire and Cable Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Excellent low temperature flexibility, lower processing temperature, and superior adhesionApplications: Flooding and f..