Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.270 MPa
39.2 psi
as received
Zircar Refractory Composites RS-3000 ALUMINA FELT
ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It..
Tensile Strength, Ultimate 0.270 MPa
39.2 psi
ASTM D3574E
Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.