Polymer Property : Tensile Strength, Ultimate = 0.159 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.159 - 59.6 MPa
23.0 - 8650 psi
Average value: 26.7 MPa Grade Count:20
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..