Polymer Property : Tensile Strength, Ultimate = 0.0700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.0700 MPa
10.2 psi
Pyrotek O-1 Low-Temperature Felt
Excellent resistance to vibration. Not effected by 1.55 MPa steam.Dimensions1524 mm x 22.9 m 6, 13, 25 mm thickApplicationsHigh-density gaskets at elevated temperatures Initial systems, high pressu..