Polymer Property : Tensile Strength, Ultimate = 0.0221 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.0221 MPa
3.20 psi
Dow Corning 9601 TEXTILE PRINTING INK
Specifically for fluorosilicone peroxide cured rubber adhesion to generic metals, glass, fabrics, and ceramicsInformation provided by Dow Corning