Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 13.0 J | 9.58 ft-lb | ASTM D3029 |
Total PSI 844E Polystyrene Polystyrene 844E is a high impact polystyrene specially designed for the custom sheet market. The polymer produces tough ductile sheet with a rich matte finish. 844E is specially formulated to minim.. |