Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 9.60 J | 7.08 ft-lb | ASTM D3763 |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Falling Dart Impact | 9.60 J | 7.08 ft-lb | ASTM D3763 |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Falling Dart Impact | 9.60 J | 7.08 ft-lb | 73°F; ASTM D3029 |
Spartech Korad® SP-2011 Cap/HIPS Polystyrene Sheet Description: Polystyrene SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |