Polymer Property : Falling Dart Impact = 624 J
Polymer Property :
Falling Dart Impact =
624 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Falling Dart Impact
624
J
460
ft-lb
73°F; NBS PS-31-70
Spartech Litho SP-2090 Polystyrene Sheet
Description: Polystyrene SheetInformation provided by Spartech.