Polymer Property : Falling Dart Impact = 6.21 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 6.21 - 11.4 J
4.58 - 8.41 ft-lb
Average value: 8.11 J Grade Count:9
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Falling Dart Impact 6.21 J
4.58 ft-lb
ASTM D3763
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant  (discontinued **)
Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat..
Falling Dart Impact 6.21 J
4.58 ft-lb
ASTM D3763
LNP ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant  (discontinued **)
Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500.Features: Lubricated, Good Wear ResistanceForms: PelletsInformation provided by LNP, a GE Plasti..