Falling Dart Impact 75.9 - 75.9 J

@Temperature -40.0 - -40.0 °C
56.0 - 56.0 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 75.9 J Grade Count:1
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..