Mechanical Properties Metric English Comments
Falling Dart Impact 51.5 J

@Temperature -28.9 °C
38.0 ft-lb

@Temperature -20.0 °F
ASTM D3763
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..