Mechanical Properties Metric English Comments
Falling Dart Impact 542.328 - 542.328 J

@Temperature -40.0 - -40.0 °C
400.001 - 400.001 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 542 J Grade Count:1
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..