Polymer Property : Falling Dart Impact = 4.07 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 4.07 J

@Temperature -40.0 °C
3.00 ft-lb

@Temperature -40.0 °F
ASTM D3029
Spartech SP-9080 High Heat ABS Sheet
Description: ABS SheetInformation provided by Spartech.