Polymer Property : Falling Dart Impact = 31.2 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 2.26 - 31.2 J
1.67 - 23.0 ft-lb
Average value: 14.2 J Grade Count:23
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..