Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J | 24.0 ft-lb | ASTM D3029 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Falling Dart Impact | 32.5 J @Temperature -40.0 °C |
24.0 ft-lb @Temperature -40.0 °F |
F50; ASTM D3029 |
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of.. |