Falling Dart Impact 4.06746 - 31.1839 J

@Temperature -40.0 - -40.0 °C
3.00000 - 23.0000 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 14.6 J Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..