Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 4.90 - 21.4 J | 3.61 - 15.8 ft-lb | Average value: 9.18 J Grade Count:17 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |