Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 197 J @Temperature -40.0 °C |
145 ft-lb @Temperature -40.0 °F |
ASTM D5420 |
Spartech Royalstatâ„¢ R632 ABS/PVC Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |