Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 11.6 - 18.4 J | 8.56 - 13.6 ft-lb | Average value: 15.9 J Grade Count:6 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |