Mechanical Properties Metric English Comments
Falling Dart Impact 24.0 J
17.7 ft-lb
-20°F, Peak Energy; ASTM D3763
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Falling Dart Impact 24.0 J
17.7 ft-lb
-29°F, Peak Energy; ASTM D3763
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010