Mechanical Properties Metric English Comments
Falling Dart Impact 18.6 J
13.7 ft-lb
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..