Mechanical Properties Metric English Comments
Falling Dart Impact 8.70 - 13.7 J
6.42 - 10.1 ft-lb
Average value: 12.0 J Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..